Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 11.1 MPa @Temperature 80.0 °C |
1610 psi @Temperature 176 °F |
Double Lap Shear; Dry; 20 min @ 175°C; Hexcel IS202 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |
|||
Shear Strength | 11.1 MPa @Temperature 80.0 °C |
1610 psi @Temperature 176 °F |
Tube Shear; Dry; 60 min @ 120°C; EN2667-2 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |