Polymer Property : Shear Strength = 1110 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 7.62 MPa

@Temperature 80.0 °C
1110 psi

@Temperature 176 °F
Tube Shear; Dry; 20 min @ 175°C; EN2667-2
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic..
Shear Strength 7.65 MPa

@Temperature 23.0 °C
1110 psi

@Temperature 73.4 °F
Overlap, Polyacrylic
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..