Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 11600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 80.0 MPa

@Temperature -53.9 °C
11600 psi

@Temperature -65.0 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Shear Strength 80.0 MPa

@Temperature 82.2 °C
11600 psi

@Temperature 180 °F
0° Short Beam, Wet
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Information provided by HexCel
Shear Strength 80.0 MPa

@Temperature 25.0 °C
11600 psi

@Temperature 77.0 °F
0° Short Beam, Wet
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber
Information provided by HexCel
Shear Strength 80.0 MPa

@Temperature 22.8 °C
11600 psi

@Temperature 73.0 °F
ILSS Weft; 10 min @ 250°F
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle
Information provided by HexCel
Shear Strength 80.0 MPa

@Temperature 22.8 °C
11600 psi

@Temperature 73.0 °F
ILSS Weft; 15 min @ 250°F
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle
Information provided by HexCel
Shear Strength 80.0 MPa

@Temperature 22.8 °C
11600 psi

@Temperature 73.0 °F
ILSS Weft; 30 min @ 250°F
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle
Information provided by HexCel
Shear Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
0º Interlaminar Shear, 120°C Cure, Conditioning: 23°C; ASTM D2344
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
1947 - 38% resin weight with M46J 52.5% fiber volumeInformation provided by HexCel
Shear Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel