Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 125 MPa @Temperature 21.1 °C |
18100 psi @Temperature 70.0 °F |
Beam, V-Notched; Dry; Autoclave Cured; ASTM D5379-93 |