Polymer Property : Shear Strength = 133 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 133 MPa

@Temperature 23.0 °C
19300 psi

@Temperature 73.4 °F
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel