Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 14.1 MPa @Temperature 149 °C |
2050 psi @Temperature 300 °F |
ASTM D732 |
Greene Tweed Avalon® 89 PTFE Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Shear Strength | 14.1 MPa @Temperature 204 °C |
2050 psi @Temperature 400 °F |
ASTM D732 |
Greene Tweed Avalon® 89 PTFE Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |