Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 103 MPa @Temperature 82.2 °C |
14900 psi @Temperature 180 °F |
Beam, V-Notched; Dry; Autoclave Cured; ASTM D5379-93 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 103 MPa @Temperature 23.0 °C |
14900 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 103 MPa @Temperature 23.0 °C |
14900 psi @Temperature 73.4 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/AS7 GS Fiber: AS7 GS, UD, 150 g/m2Information provided by HexCel |
|||
Shear Strength | 103 MPa @Temperature 23.0 °C |
14900 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |