Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 111 MPa @Temperature 24.0 °C |
16100 psi @Temperature 75.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel |
|||
Shear Strength | 111 MPa @Temperature 23.0 °C |
16100 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 111 MPa @Temperature 24.0 °C |
16100 psi @Temperature 75.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T095 Carbon Tape Hexcel designation: T_095-12"-F263; Various fibersInformation provided by HexCel |