Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 17.00 MPa @Temperature 100 °C |
2465 psi @Temperature 212 °F |
Lap Shear |
Hexcel® Redux® 610W (0.03 psf) Flame retarded epoxy film adhesive Redux 610 is a modified, flame-retarded epoxy film adhesive curing at 250°F. It is suitable for bonding metal to metal and for sandwich structures where flame retardancy and low heat release are re.. |
|||
Shear Strength | 17.00 MPa @Temperature 149 °C |
2465 psi @Temperature 300 °F |
Lap Shear |
Hexcel® Redux® 641K Modified epoxy film adhesive for bonding metallic and composite components Redux 641 is a high temperature modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures where operating temperatures are experienced up t.. |