Polymer Property : Shear Strength = 17000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 117 MPa

@Temperature 25.0 °C
17000 psi

@Temperature 77.0 °F
In-Plane +/- 45 tensile shear; Dry
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Information provided by HexCel