Mechanical Properties Metric English Comments
Shear Strength 12.8 MPa

@Temperature 65.6 °C
1850 psi

@Temperature 150 °F
ASTM D732
Greene Tweed Avalon® 56 PTFE
PTFE is used in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use..