Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.14 MPa @Temperature 25.0 °C |
310 psi @Temperature 77.0 °F |
Tensile, Al/Al lap joint; cured 90 days @ 25°C |
Abatron AboCast 8110-1/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Shear Strength | 2.14 MPa @Temperature 82.0 °C |
310 psi @Temperature 180 °F |
Overlap, PVC |
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |