Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 21.2 MPa @Temperature 0.000 °C |
3080 psi @Temperature 32.0 °F |
Tensile, Al/Al lap joint; cured 2 hours @ 93°C |
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |