Mechanical Properties Metric English Comments
Shear Strength 26.5 MPa

@Temperature 25.0 °C
3840 psi

@Temperature 77.0 °F
Bond; Aluminum to aluminum, 1" overlap
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive
Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther..