Shear Strength 27.4 MPa

@Temperature 0.000 °C
3980 psi

@Temperature 32.0 °F
Tensile, Al/Al lap joint; cured 2 hours @ 93°C
Abatron AboCast 8110-8/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..