Polymer Property : Shear Strength = 2940 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 20.3 MPa

@Temperature 23.9 °C
2940 psi

@Temperature 75.0 °F
– 6061-T6 Aluminum (abraded), with Arovex Carbon Fiber Epoxy Laminate
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid
Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods..