Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 30.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.207 MPa

@Temperature 22.2 °C
30.0 psi

@Temperature 72.0 °F
Lap Shear Unprimed, 12 months at 300°F
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf)
Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve..
Shear Strength 0.207 MPa

@Temperature 107 °C
30.0 psi

@Temperature 225 °F
Overlap, 1/8 birch to 1/8 birch, bond tested after aging 3 weeks @ 24°C and 50% RH at a separation rate of 0.2 in/min; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 0.207 MPa

@Temperature 93.0 °C
30.0 psi

@Temperature 199 °F
Overlap, 1/8" birch 1/8" birch
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Shear Strength 0.207 MPa

@Temperature 82.0 °C
30.0 psi

@Temperature 180 °F
1/8" Birch/High-Pressure Laminate, no aging
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Shear Strength 0.207 MPa

@Temperature 150 °C
30.0 psi

@Temperature 302 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.207 MPa

@Temperature 150 °C
30.0 psi

@Temperature 302 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.207 MPa

@Temperature 107 °C
30.0 psi

@Temperature 225 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.207 MPa

@Temperature 107 °C
30.0 psi

@Temperature 225 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.207 MPa

@Temperature 93.0 °C
30.0 psi

@Temperature 199 °F
Overlap, 1/8" birch 1/8" birch
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Shear Strength 0.207 MPa

@Temperature 82.0 °C
30.0 psi

@Temperature 180 °F
1/8" Birch/High-Pressure Laminate, no aging
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Copyright © lookpolymers.com All Rights Reserved