Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 30.74 MPa @Temperature 21.1 °C |
4459 psi @Temperature 70.0 °F |
Cure Cycle, 6 hrs @ 220°F, FPL Acid Etched 6061-T6, Std Dev 134; ASTM D1002 |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |