Polymer Property : Shear Strength = 31.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 31.7 MPa

@Temperature 93.3 °C
4600 psi

@Temperature 200 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Shear Strength 31.7 MPa

@Temperature 79.4 °C
4600 psi

@Temperature 175 °F
Lap Shear
Hexcel® Redux® 312 Modified epoxy film adhesive (0.015 psf)
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Shear Strength 31.7 MPa

@Temperature 71.1 °C
4600 psi

@Temperature 160 °F
Lap Shear
Hexcel® Redux® 312UL Modified epoxy film adhesive
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Shear Strength 31.7 MPa

@Temperature 79.4 °C
4600 psi

@Temperature 175 °F
Lap Shear
Hexcel® Redux® 312UL Modified epoxy film adhesive
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..