Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 32.1 MPa @Temperature 24.0 °C |
4650 psi @Temperature 75.2 °F |
with Scotch-Weld EW-5000, 14 days at 71°C and 95% RH; ASTM D1002-10 |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |