Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 23.4 MPa @Temperature 71.0 °C |
3400 psi @Temperature 160 °F |
with Scotch-Weld EW-5000; ASTM D1002-10 |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |
|||
Shear Strength | 23.4 MPa @Temperature 71.0 °C |
3400 psi @Temperature 160 °F |
No Primer; ASTM D1002-10 |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |