Mechanical Properties Metric English Comments
Shear Strength 37.80 MPa

@Temperature 60.0 °C
5482 psi

@Temperature 140 °F
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-1
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and ..