Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 39.0 MPa

@Temperature 177 °C
5660 psi

@Temperature 351 °F
T300; Fill Short Beam; Wet condition
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel
Shear Strength 39.0 MPa

@Temperature 100 °C
5660 psi

@Temperature 212 °F
Interlaminar shear
Hexcel® HexPly® M36/NC2 180°C (350°F) Curing Epoxy Matrix, Multiaxial Fabric Laminate (NC2)
Uses Hexcel NC2 non-crimp fabric based on Tenax HTS fiber; Quasi-isotropic lay-up based on 1072 gsm quadaxial NC2 fabric (267 gsm/ply); Laminates manufactured via resin film infusionInformation prov..
Shear Strength 39.0 MPa

@Temperature 60.0 °C
5660 psi

@Temperature 140 °F
0º Interlaminar Shear, Conditioning: 60°C-90%RH; ASTM D2344
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel