Mechanical Properties Metric English Comments
Shear Strength 0.3325 MPa

@Shear Rate 5000 1/s,
Temperature 270 °C
48.23 psi

@Shear Rate 5000 1/s,
Temperature 518 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers