Polymer Property : Shear Strength = 4800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 33.1 MPa

@Temperature 177 °C
4800 psi

@Temperature 350 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Shear Strength 33.1 MPa

@Temperature 177 °C
4800 psi

@Temperature 350 °F
Wet (140°F/95% RH), In-plane; ASTM D3846
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) 6781 S2 Glass Fabric
Developed using state-of-the-art formulating technologies, RM-3000 One Part BMI RTM Resin delivers superior hot/wet performance in airframe, missile and propulsion applications at service temperatu..
Shear Strength 33.1 MPa

@Temperature 175 °C
4800 psi

@Temperature 347 °F
Laminate property; In Line Shear; Conditioning: 14 days Water 158°F
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l..
Shear Strength 33.1 MPa

@Temperature 71.1 °C
4800 psi

@Temperature 160 °F
Lap Shear
Hexcel® Redux® 312 Modified epoxy film adhesive (0.015 psf)
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Shear Strength 33.1 MPa

@Temperature 21.1 °C
4800 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..