Polymer Property : Shear Strength = 57.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 57.0 MPa

@Temperature 50.0 °C
8270 psi

@Temperature 122 °F
ILSS Weft; 30 min @ 250°F
Hexcel® HexPly® EF02 Epoxy Curing System after THR 120 EF01 S50 37% Curing Cycle
Information provided by HexCel
Shear Strength 57.0 MPa

@Temperature 177 °C
8270 psi

@Temperature 351 °F
Short Beam; Autoclave Cured; [0°]16; Wet condition
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form
Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel
Shear Strength 57.0 MPa

@Temperature 90.0 °C
8270 psi

@Temperature 194 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel