Polymer Property : Shear Strength = 5945 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 40.99 MPa

@Temperature -55.0 °C
5945 psi

@Temperature -67.0 °F
Lap Shear
Hexcel® Redux® 641K Modified epoxy film adhesive for bonding metallic and composite components
Redux 641 is a high temperature modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures where operating temperatures are experienced up t..