Mechanical Properties Metric English Comments
Shear Strength 6.30 MPa

@Temperature 22.0 °C
914 psi

@Temperature 71.6 °F
Short Beam Shear; Dry; 30 min @ 150°C; DMS2180
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic..
Shear Strength 6.30 MPa

@Temperature 22.0 °C
914 psi

@Temperature 71.6 °F
Short Beam Shear; Dry; 20 min @ 175°C; DMS2180
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic..