Mechanical Properties Metric English Comments
Shear Strength 68.1 MPa

@Temperature 50.0 °C
9870 psi

@Temperature 122 °F
ILSS Weft; 15 min @ 250°F
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle
Information provided by HexCel
Shear Strength 68.1 MPa

@Temperature 50.0 °C
9870 psi

@Temperature 122 °F
ILSS Weft; 30 min @ 250°F
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle
Information provided by HexCel