Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 76.0 MPa @Temperature 132 °C |
11000 psi @Temperature 270 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T190 Carbon Tape Hexcel designation: T_190-12"-F263; Various fibersInformation provided by HexCel |