Mechanical Properties Metric English Comments
Shear Strength 8.27 - 8.62 MPa

@Temperature -55.0 °C
1200 - 1250 psi

@Temperature -67.0 °F
Overlap Al/Al (etched); ASTM D1002-72
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Shear Strength 8.27 - 8.62 MPa

@Temperature -55.0 °C
1200 - 1250 psi

@Temperature -67.0 °F
Overlap Al/Al (etched); ASTM D1002-72
3M Scotch-Weld™ DP270 Clear Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M