Polymer Property : Shear Strength = 8.998 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 8.998 MPa

@Temperature 22.2 °C
1305 psi

@Temperature 72.0 °F
Aluminum Double Lap Shear (0.06 inch gap)
Hexcel® Redux® 219/2-NA Foaming adhesive film
The Redux 200 series is a range fo foaming adhesive films presented in sheet form. They expand during the cure cycle to fill gaps and adhere strongly to all parts of the structure with which they co..
Shear Strength 8.998 MPa

@Temperature 25.0 °C
1305 psi

@Temperature 77.0 °F
Tensile, Al/Al lap joint; cured 2 hours @ 93°C
Abatron AboCast 8110-4/AboCure 8110-3 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..