Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.00 MPa @Temperature 149 °C |
870 psi @Temperature 300 °F |
Aluminum Double Lap Shear (0.06 inch gap) |
Hexcel® Redux® 219/3-NA Foaming adhesive film The Redux 200 series is a range fo foaming adhesive films presented in sheet form. They expand during the cure cycle to fill gaps and adhere strongly to all parts of the structure with which they co.. |
|||
Shear Strength | 6.00 MPa @Temperature 82.0 °C |
870 psi @Temperature 180 °F |
Overlap, FRP |
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |