Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.621 MPa

@Temperature 23.0 °C
90.0 psi

@Temperature 73.4 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.621 MPa

@Temperature 23.0 °C
90.0 psi

@Temperature 73.4 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..