Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.275 GPa

@Temperature 120 °C
39.9 ksi

@Temperature 248 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Shear Modulus 0.275 GPa

@Temperature 120 °C
39.9 ksi

@Temperature 248 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..