Polymer Property : Shear Modulus = 0.287 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.287 GPa

@Temperature 120 °C
41.6 ksi

@Temperature 248 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..