Mechanical Properties Metric English Comments
Shear Modulus 0.306 GPa

@Temperature 110 °C
44.4 ksi

@Temperature 230 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..