Mechanical Properties Metric English Comments
Shear Modulus 0.4832 GPa

@Temperature 70.0 °C
70.08 ksi

@Temperature 158 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..