Polymer Property : Shear Modulus = 0.524 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.524 GPa

@Temperature 160 °C
76.0 ksi

@Temperature 320 °F
DAM; ISO 6721
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Shear Modulus 0.524 GPa

@Temperature 160 °C
76.0 ksi

@Temperature 320 °F
DAM; ISO 6721
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Shear Modulus 0.524 GPa

@Temperature 160 °C
76.0 ksi

@Temperature 320 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..