Mechanical Properties Metric English Comments
Shear Modulus 1.576 GPa

@Temperature 70.0 °C
228.6 ksi

@Temperature 158 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and..