Polymer Property : Shear Modulus = 1.60 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.60 GPa

@Temperature 50.0 °C
232 ksi

@Temperature 122 °F
DAM; ISO 6721
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Shear Modulus 1.60 GPa

@Temperature 177 °C
232 ksi

@Temperature 351 °F
AS4C; In Plane; Wet condition
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel