Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.867 GPa @Temperature 70.0 °C |
270.8 ksi @Temperature 158 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |