Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.812 GPa @Temperature 120 °C |
118 ksi @Temperature 248 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Shear Modulus | 0.817 GPa @Temperature 70.0 °C |
118 ksi @Temperature 158 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |