Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.963 GPa @Temperature 10.0 °C |
140 ksi @Temperature 50.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |