Polymer Property : Shear Modulus = 144.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.9984 GPa

@Temperature -20.0 °C
144.8 ksi

@Temperature -4.00 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers