Polymer Property : Shear Modulus = 157 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.08 GPa

@Temperature -20.0 °C
157 ksi

@Temperature -4.00 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..