Polymer Property : Shear Modulus = 2.604 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 2.604 GPa

@Temperature -50.0 °C
377.7 ksi

@Temperature -58.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)