Shear Modulus 1.54 GPa

@Temperature 20.0 °C
223 ksi

@Temperature 68.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..