Mechanical Properties Metric English Comments
Shear Modulus 1.5884 GPa

@Temperature 10.0 °C
230.38 ksi

@Temperature 50.0 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope..