Mechanical Properties Metric English Comments
Shear Modulus 1.974 GPa

@Temperature 20.0 °C
286.3 ksi

@Temperature 68.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET)
Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers